Partial renewed formation of pearlite - 1.3505

Treatment :  spheroidised
Magnification :  200 : 1
Etching medium :  3 % alcoholic nitric acid
Sampling / Specification :  transverse
Testing result :

partial renewed formation of pearlite

caused by surface decarburization

Treatment :  spheroidised
Magnification :  500 : 1
Etching medium :  3 % alcoholic nitric acid
Sampling / Specification :  transverse
Testing result :

partial renewed formation of pearlite

caused by surface decarburization