Strong carbide precipitate - 1.4310

 

If austenitic material isn't quenched into water after the solution annealing or after the hot forming, carbide precipitate can precipitate themselves on the grain boundaries. The higher the carbon amount is in the steel, the more precipitate can be available.

Rod wire 10,00 mm round - untreated

Back to material defects

 