Bad heat treated structure - 1.7225

Treatment :  quenched and tempered
Magnification :  100 : 1
Etching medium :  3 % alcoholic nitric acid
Sampling / Specification :  longitudinal
Testing result :

heat treated structure with bainite transformation

Treatment :  quenched and tempered
Magnification :  200 : 1
Etching medium :  3 % alcoholic nitric acid
Sampling / Specification :  longitudinal
Testing result :

heat treated structure with bainite transformation