Microstructure deformation by scalping - 1.7076

Treatment :  untreated
Magnification :  200 : 1
Etching medium :  3 % alcoholic nitric acid
Sampling / Specification :  transverse
Testing result :

zone with microstructure deformation 0,03 mm deep

Treatment :  untreated
Magnification :  500 : 1
Etching medium :  3 % alcoholic nitric acid
Sampling / Specification :  transverse
Testing result :

zone with microstructure deformation 0,03 mm deep

previous page

back to material defects

 

next page