Treatment : spheroidised
Magnification : 100 : 1
Etching medium : 3 % alcoholic nitric acid
Sampling / Specification : transverse
Testing result :
carburization 0,14 mm deep |
Treatment : spheroidised
Magnification : 200 : 1
Etching medium : 3 % alcoholic nitric acid
Sampling / Specification : transverse
Testing result :
carburization 0,14 mm deep
complete decarburization and
grain boundary oxidation 0,01 mm deep |