Fracture through sigma-phase - 1.4462

 

The sigma-phase is a brittle, intermetallic phase with high hardness. The sigma-phase is very brittle and has a bad impact strength. For this reason material with sigma phase can be usually bad or not processed. In this case it came to fractures at the cold rolling.

Rod wire 11,00 mm round - solution annealed

Back to material defects

 