Shrink hole with scale - 1.2343

 

Shrink holes in the steel appear, if after the casting cavities, which cannot be closed at the further reforming, are in the ingot or the strand. On the one hand, too low reformings and on the other hand scale or slag in the cavity can prevent a welding together during the hot forming.

Rod wire 10,00 mm round - pickled , annealed