Pores in the core - 1.2379

 

Pores and discontinuity in the steel, which cannot be closed at the further reforming, appear if cavities are in the ingot or strand after the casting. Another cause can be, that melting on and internal bursts result by the hot forming by too high core temperatures in the rolling piece or forging piece.