Burst open upsetting sample - 1.4301

Treatment :  solution annealed
Magnification :  6,5 : 1
Etching medium :  
Sampling / Specification :  surface of upsetting sample
Testing result :

strong burst open upsetting sample

Treatment :  solution annealed
Magnification :  50 : 1
Etching medium :  
Sampling / Specification :  transverse
Testing result :

pincher 0,31 mm deep as the cause of defect