Stress crack at the wire - 1.7707

Treatment :  quenched and tempered
Magnification :  2 : 1
Etching medium :  
Sampling / Specification :  wire surface
Testing result :

longitudinal defects on the surface

Treatment :  quenched and tempered
Magnification :  6,5 : 1
Etching medium :  
Sampling / Specification :  wire surface
Testing result :

longitudinal defects on the surface

previous page

back to material defects

 

next page