Strong slag line - 1.4718

 

Non metallic inclusions (slags), branch-on through the casting process, can occur in the steel. If slag is washed in larger quantity into the steel by an irregularity during the cast, these non metallic inclusions in the material can be existing as long lines, after rolling the pre-material. The size of this slag line is dependent on the slag amount in the pre-material and on the reforming of the rolled piece.

Rod wire 11,00 mm round - quenched and tempered

Back to material defects

 