Stress crack on the rod wire - 1.8523

Treatment :  spheroidised
Magnification :  200 : 1
Etching medium :  
Sampling / Specification :  transverse
Testing result :

stress crack arisen at the cooling of the rod wire, before
the annealing ; defect depth 0,17 mm

Treatment :  spheroidised
Magnification :  500 : 1
Etching medium :  
Sampling / Specification :  transverse
Testing result :

stress crack arisen at the cooling of the rod wire, before
the annealing ; defect depth 0,17 mm
light scaled surroundings of the defect