Hardening stress crack - 1.7035

Treatment :  quenched and tempered
Magnification :  12,5 : 1
Etching medium :  
Sampling / Specification :  transverse
Testing result :

hardening stress crack 2,65 mm deep

Treatment :  quenched and tempered
Magnification :  100 : 1
Etching medium :  
Sampling / Specification :  transverse
Testing result :

hardening stress crack
with scaled crack configuration