Stress crack - 1.8519

Treatment :  quenched and tempered
Magnification :  12,5 : 1
Etching medium :  
Sampling / Specification :  transverse
Testing result :

stress crack 1,80 mm deep

Treatment :  quenched and tempered
Magnification :  200 : 1
Etching medium :  
Sampling / Specification :  transverse
Testing result :

scaled crack configuration and scaled crack edges

with grain boundary oxidation

previous page

back to material defects

 

next page