The following examinations were carried out at a welded seam
laid out for education purposes . The initial material was ca. 20 mm thick and
the materail number is 1.0501 (C35) . The examinations from microstructure and
hardness are realized at 9 testing areas . After the welding the material became
no heat treatment subjected . In the general the crystalline structure formation
and change through the heat effect of the different weld positions shall be represented
.