Material number 1.1122     -     CQ10 / C10C / C10E2C

 
Composition in % :

C

Si

Mn

P

S

Cr

Mo

Ni

0,07 - 0,13

0,15 - 0,35

0,25 - 0,50

max. 0,035

max. 0,035

 

 

 

V

W

Ti

Cu

Al

Nb

B

N

 

 

 

 

 

 

 

 


Range of application and heat treatment :

Cold extrusion steel : universal machines- , engines- and vehicle engineering 
Hardening : 880 - 920 °C (water)          Soft annealing : 650 - 700 °C          Normalising : 880 - 920 °C 

General and distinctive features :

 
 

Material selection

Analyses selection