Composition in % :
|
C |
Si |
Mn |
P |
S |
Cr |
Mo |
Ni |
|
0,12 - 0,18 |
max. 0,40 |
0,30 - 0,60 |
max. 0,035 |
0,020 - 0,040 |
|
|
|
Range of application and heat treatment :
|
Cementation steel : for structural- and machine components
- pins , boxes , lever
Hardening : 880 - 920 °C (water) Soft
annealing : 650 - 700 °C Normalising
: 880 - 920 °C |
General and distinctive features :
|