Material number 1.1191     -     Ck45 / C45E

 
Composition in % :

C

Si

Mn

P

S

Cr

Mo

Ni

0,42 - 0,50

max. 0,40

0,50 - 0,80

max. 0,035

max. 0,030

 

 

 

V

W

Ti

Cu

Al

Nb

B

N

 

 

 

 

 

 

 

 


Range of application and heat treatment :

Heat treatable steel / Structural steel : components for middle strain - higher purity degree requirements 
Hardening : 820 - 860 °C (oil or water)          Soft annealing : 650 - 700 °C          Normalising : 840 - 880 °C 