Treatment : untreated
Magnification : 100 : 1
Etching medium : 3 % alcoholic nitric acid
Sampling / Specification : transverse
Testing result :
surface decarburization 0,20 mm deep |
Treatment : untreated
Magnification : 200 : 1
Etching medium : 3 % alcoholic nitric acid
Sampling / Specification : transverse
Testing result :
ca. 40 % ferrite ; 50 % pearlite ; 10 % sorbite
|