Material number 1.1249     -     Cf70 / C70G

 
Composition in % :

C

Si

Mn

P

S

Cr

Mo

Ni

0,68 - 0,75

0,15 - 0,35

0,20 - 0,35

max. 0,025

max. 0,035

 

 

 

V

W

Ti

Cu

Al

Nb

B

N

 

 

 

 

 

 

 

max. 0,007


Range of application and heat treatment :

Heat treatable steel for surface hardening : worm gearing , piston bolts , camshafts , lathe spindles 
Hardening : 790 - 820 °C (water)          Soft annealing : 650 - 700 °C          Normalising : 820 - 850 °C 