Material number 1.1563     -     C125W / C125U

 
Composition in % :

C

Si

Mn

P

S

Cr

Mo

Ni

1,20 - 1,35

0,10 - 0,30

0,10 - 0,35

max. 0,030

max. 0,030

 

 

 

V

W

Ti

Cu

Al

Nb

B

N

 

 

 

 

 

 

 

 


Range of application and heat treatment :

Unalloyed Tool steel : scraper , cutter blade , file , knife 
Hardening : 760 - 790 °C (water)          Soft annealing : 680 - 710 °C 