Material number 1.1740     -     C60W / C60U

 
Composition in % :

C

Si

Mn

P

S

Cr

Mo

Ni

0,55 - 0,65

0,15 - 0,40

0,60 - 0,80

max. 0,035

max. 0,035

 

 

 

V

W

Ti

Cu

Al

Nb

B

N

 

 

 

 

 

 

 

 


Range of application and heat treatment :

Unalloyed Tool steel : shanks for hard metal tools , stone hammers , wood saws , pincers 
Hardening : 800 - 830 °C (oil)          Soft annealing : 680 - 710 °C 

General and distinctive features :

 
 