Composition in % :
|
C |
Si |
Mn |
P |
S |
Cr |
Mo |
Ni |
|
0,35 - 0,45 |
0,30 - 0,50 |
1,40 - 1,60 |
max. 0,030 |
0,05 - 0,10 |
1,80 - 2,00 |
0,15 - 0,25 |
|
Range of application and heat treatment :
|
Tool steel for cold working : tools for plastics processing
, good cutting properties
Hardening : 830 - 870 °C (oil) Soft
annealing : 760 - 780 °C |
General and distinctive features :
|