Material number 1.2316     -     X36CrMo17 / X38CrMo16

 
Composition in % :

C

Si

Mn

P

S

Cr

Mo

Ni

0,33 - 0,43

max. 1,00

max. 1,00

max. 0,030

max. 0,030

15,00 - 17,00

1,00 - 1,30

max. 1,00

V

W

Ti

Cu

Al

Nb

B

N

 

 

 

 

 

 

 

 


Range of application and heat treatment :

Tool steel for cold working : corrosion resistant dies 
Hardening : 1000 - 1040 °C (oil)          Soft annealing : 780 - 820 °C 

General and distinctive features :

 
 